Ammoxidation Catalyst (titanium Silicon Molecular Sieve TS-1)

Ammoxidation Catalyst (titanium Silicon Molecular Sieve TS-1)

Ammoxidation catalyst has a three-dimensional pore structure is composed of two sets of ten membered ring channel and a set of ninemembered ring channel interleaving composition, molar group hasbecome (0.001 ~ 0.2) TiO2: SiO2. Ammoxidation catalyst is Ti atoms replace part of aluminum atoms...

Description

Ammoxidation catalyst (titanium silicon molecular sieve TS-1).jpg

Ammoxidation catalyst has a three-dimensional pore structure is composed of two sets of ten membered ring channel and a set of ninemembered ring channel interleaving composition, molar group hasbecome (0.001 ~ 0.2) TiO2: SiO2.

Ammoxidation catalyst is Ti atoms replace part of aluminum atoms insilicon aluminium molecular sieve and into, which belongs to ZSM-5 series zeolite molecular sieve, with the MFI structure, composed ofsilicon oxygen tetrahedron and titanium oxygen tetrahedron primarystructural unit, connecting through the oxygen bridge, constitute asecondary structure unit of five membered rings, and further to form a three-dimensional porous skeleton, pore structure with two-dimensional MFI molecular sieve, parallel to the a axis of the ten membered ring is in a S shape, aperture of 0.51nm * 0.55nm, ten membered ring and linearly parallel to the b axis direction,aperture of 0.54nm * 0.56nm.

Use:

Ammoxidation catalyst is produced by our company, the averagediameter of 50-60m, minimum close to 10m, the maximum is less than 105m, uniform particle size distribution.

Ammoxidation catalyst can be used as catalytic oxidation catalyst,is widely used in oxidation, epoxidation and amidoximation reaction.For example, a catalyst for the production of propylene oxide,catalyst for the production of cyclohexanone oxime.

Ammoxidationcatalyst TS-1 titanium silicon molecular sieve

Index

Unit

Figure

Index of single digit SiO2/TiO2

The molar ratio

25-40

The sodium content of

Wt%

0.01%

The grain size of

um

0.2-0.4

Bulk Density

g/ml

0.55±0.1

specific surface area g

m2/g

≥450

Water content

Wt%

< 2%

Packing

Bag/drum

25kg

The reaction performance of amine oxime

Raw material conversion rate %

≥99.9%

The epoxidation reaction performance%

≥99%

The one-way service life

≥240hour

The total life

≥3000hour

The properties of epoxy reaction

The epoxidation reaction performance%

≥99.9%

Product selectivity %

≥95%

Life

≥400hour

Quality Control.jpgquality.jpg


Lushun Huitong is one of the professional ammoxidation catalyst (titanium silicon molecular sieve ts-1) manufacturers and suppliers in China, welcome to buy ammoxidation catalyst (titanium silicon molecular sieve ts-1) from our factory.
Hot Tags: ammoxidation catalyst (titanium silicon molecular sieve ts-1) China, manufacturers, suppliers, factory, buy
Related Products

Feedback